Uniform Deposition of Li-Metal Anodes Guided by 3D Current Collectors with In Situ Modification of the Lithiophilic Matrix
Chenyi Sun,Yinghui Yang,Xiufang Bian,Rongzhang Guan,Chao Wang,Dujiang Lu,Li Gao,Dongmei Zhang
DOI: https://doi.org/10.1021/acsami.1c13896
2021-10-07
Abstract:The lithium (Li)-metal anode is deemed as the "holy gray" of the next-generation Li-metal system because of its high theoretical specific capacity, minimal energy density, and lowest standard electrode potential. Nevertheless, its commercial application has been limited by the large volume variation during charge and discharge, the unstable interface between the Li metal and electrolyte, and uneven deposition of Li. Herein, we present a 3D host (Cu) with lithiophilic matrix (CuO and SnO2) in situ modification via a facile ammonia oxidation method to serve as a current collector for the Li-metal anode. The 3D Cu host embellished by CuO and SnO2 is abbreviated as 3D CSCC. By increasing interfacial activity, lowering the nucleation barrier, and accommodating changes in volume of the Li metal, the 3D CSCC electrode effectively demonstrates a homogeneous and dendrite-free deposition morphology with an excellent cycling performance up to 3000 h at a 1.0 mA cm–2 current density. Additionally, the full cells paired with CSCC anodes and LiCoO2 cathodes show good capacity retention performance at 0.2 C.The Supporting Information is available free of charge at https://pubs.acs.org/doi/10.1021/acsami.1c13896.XPS survey spectrum of 3D CSCC; EDS mapping images of 3D CSCC; SEM images of various amounts of Li plating in 3D CSCC with a current density of 1.0 mA cm-2; SEM images of various amounts of Li stripping in Cu foil with a current density of 1.0 mA cm-2; SEM images of various amounts of Li stripping in 3D CSCC with a current density of 1.0 mA cm-2; plating/stripping SEM images of 10 and 50 cycles in 3D CSCC at a current density of 1.0 mA cm-2 with a density of 1.0 mA h cm-2; 10th, 50th, 100th, and 200th circles of voltage profiles of Li plating/stripping on 3D CSCC at a current density of 0.5 mA cm-2 with a capacity of 0.5 mA h cm-2; voltage–time profiles of the Li-plated plane 3D CSCC and the Cu foil current collector Li||Li symmetric cell; detailed voltage profiles of 3D CSCC and the Cu foil current collector electrodes in symmetric cells at a current density of 1.0 mA cm-2 with a capacity of 1.0 mA h cm-2; voltage profiles of the Li-plated CSCC||Li symmetric cell at increasing current densities from 0.5 to 1.0, 2.0, and 4.0 mA cm-2 for a 1.0 mA h cm-2 capacity; cycling performances of LCo|| CSCC cells at a rate of 1 C and 2 C; EIS of 3D CSCC and the Cu foil current collector in different electrolytes; and voltage profiles of Li plating on 3D CSCC with a capacity of 1.0 mA h cm-2 at a current density of 1.0 mA cm-2 in different electrolytes (PDF)This article has not yet been cited by other publications.
materials science, multidisciplinary,nanoscience & nanotechnology