Fretting behavior evolution of steel wires with helical structure after adding ore particles in lubricating grease

Chunming Xu,Yuxing Peng,Zhencai Zhu,Wei Tang,Kun Huang
DOI: https://doi.org/10.1016/j.engfailanal.2021.105332
IF: 4
2021-06-01
Engineering Failure Analysis
Abstract:<p>The mineral particles in the mine air aggravate the wear of wire rope, which seriously threatens the lifespan of wire rope. Therefore, the wear test of steel wires with helical structure was performed by a homemade tester. Results show that the coefficient of friction (CoF) curve under the original grease condition presents a slight increasing trend, while the CoF decreases with increasing the cycles after adding ore particles. For the grease mixed with ore particles, as the loading force increases, the wear volume of steel wire increases, while the wear coefficient shows a decreasing trend. The wear mechanism of steel wire under the original grease condition shows obvious abrasive wear and fatigue wear, while the wear mechanism under the mixed grease condition includes abrasive wear, adhesive wear and fatigue wear. Additionally, the wear characteristics of the peak friction pair are more obvious and severe than that of the valley friction pair under the mixed grease condition.</p>
engineering, mechanical,materials science, characterization & testing
What problem does this paper attempt to address?