Mitigating voltage decay of O3‐NaNi1/3Fe1/3Mn1/3O2 layered oxide cathode for sodium‐ion batteries by incorporation of 5d metal tantalum

Shuai Huang,Yuanyuan Sun,Tao Yuan,Haiying Che,Qinfeng Zheng,Yixiao Zhang,Pengzhi Li,Jian Qiu,Yuepeng Pang,Junhe Yang,Zi‐Feng Ma,Shiyou Zheng
DOI: https://doi.org/10.1002/cnl2.136
2024-05-29
Carbon Neutralization
Abstract:This study addresses the challenge of cycling stability in O3‐NaNi1/3Fe1/3Mn1/3O2 cathode for SIBs by substituting Ni/Fe/Mn with 5d metal tantalum, leading to suppressed lattice distortion. The optimized Na(Ni1/3Fe1/3Mn1/3)0.97Ta0.03O2 sample demonstrates improved reversible capacity, rate performance, voltage decay mitigation, and moisture resistance, showcasing its potential for practical utilization in energy storage applications. The cycling stability of O3‐type NaNi1/3Fe1/3Mn1/3O2 (NFM) as a commercial cathode material for sodium ion batteries (SIBs) is still a challenge. In this study, the Ni/Fe/Mn elements are replaced successfully with tantalum (Ta) in the NFM lattice, which generated additional delocalized electrons and enhanced the binding ability between the transition metal and oxygen, resulting in suppressed lattice distortion during charging and discharging. This caused significant mitigation of voltage decay and improved cycle stability within the potential range of 2.0–4.2 V. The optimized Na(Ni1/3Fe1/3Mn1/3)0.97Ta0.03O2 sample achieved a reversible capacity of 162.6 mAh g−1 at a current rate of 0.1 C and 73.2 mAh g−1 at a high rate of 10 C. Additionally, the average charge/discharge potential retention reached 98% after 100 cycles, significantly mitigating the voltage decay. This work demonstrates a significant contribution towards the practical utilization of NFM cathodes in the SIBs energy storage field.
English Else
What problem does this paper attempt to address?