Abstract:In this article, the strain limit criterion and classical strength theories are used to evaluate the strength at the cold spot with nested effect of the deformed coke drum. First, the geometric model of the cold spot with nested effect before and after the deformation of the drum wall is established in the selected area, and the nested stress at the cold spot is calculated. Then, according to the calculated stress–strain results, the stress analysis of the drum wall at the cold spot is carried out. The results show that the coke drum yields during the cooling stage according to the strain limit criterion. According to classical strength theories, coke drum yields during the coke production and cooling stages. Finally, the paths are selected to calculate the equivalent stress–strain, and the stress–strain curves along the paths are plotted. By comparing the results of stress and strain evaluation, three evaluation methods are compared and studied.
materials science, multidisciplinary,mechanics, composites, characterization & testing
What problem does this paper attempt to address?