Spontaneous In Situ Surface Alloying of Li-Zn Derived from a Novel Zn 2+ -Containing Solid Polymer Electrolyte for Steady Cycling of Li Metal Battery

Zhen Zeng,Shang Wang,Jun Cheng,Guangmei Hou,Deping Li,Guifang Han,Lijie Ci
DOI: https://doi.org/10.1021/acssuschemeng.1c00878
2021-03-09
Abstract:Solid polymer electrolytes (SPEs) are preferable in the pursuit for developing high-energy Li metal batteries due to their inherent flexibility and intimate contact with electrodes. However, continuous interfacial parasitic reactions and undesired Li dendrite growth caused by inhomogeneous plating/stripping of Li<sup>+</sup> result in rapid deterioration of an SPE/Li interface. Herein, a novel Zn<sup>2+</sup>-containing SPE (SPE-<i>x</i>Zn) with anionic groups partially tethered on the polymer chains is developed to meet these challenges. During cycling, Zn<sup>2+</sup> cations inside the SPE-<i>x</i>Zn will gradually migrate to the surface of a Li electrode and then evolve to a Li-Zn alloy layer, where Li<sup>+</sup> can diffuse more efficiently. Meanwhile, owing to the electrostatic interaction, the immobilized anionic groups within SPE-<i>x</i>Zn can alleviate local concentrated Li<sup>+</sup> flux. The synergistic effects of an in situ formed alloy layer and unique macromolecular structure can promote uniform plating/stripping of Li, thus yielding a more stable SPE-<i>x</i>Zn/Li interface. Therefore, steady cycling over 300 h at 0.2 mA cm<sup>–2</sup> is achieved by Li/SPE-5Zn/Li, and an impressive capacity retention of 87.3% at 0.5 C after 800 cycles is realized by LFP/SPE-5Zn/Li with an average Coulombic efficiency of 99.90%.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acssuschemeng.1c00878?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acssuschemeng.1c00878</a>.TGA profiles of SPE-<i>x</i>Zn Ar and N<sub>2</sub> atmospheres (Figure S1); flame tests of SPE-0Zn and SPE-5Zn (Figure S2); <i>t</i><sub>c</sub> (Figure S3) and LSV (Figure S4) tests for SPE-0Zn, SPE-2.5Zn, SPE-7.5Zn, and SPE-10Zn; cycling performance of the Li/SPE-PEO/Li cell (Figure S5); FT-IR (Figure S6) and XPS (Figure S7) for SPE-0Zn and SPE-5Zn before and after cycling; cycling performance of the LFP/SPE-PEO/Li cell (Figure S8); thickness of SPE-<i>x</i>Zn and SPE-PEO (Table S1); and ionic conductivity of SPE-<i>x</i>Zn at varying temperatures (Table S2) (<a class="ext-link" href="/doi/suppl/10.1021/acssuschemeng.1c00878/suppl_file/sc1c00878_si_001.pdf">PDF</a>)Flame tests for SPE-PEO and SPE-5Zn (Video 1) (<a class="ext-link" href="/doi/suppl/10.1021/acssuschemeng.1c00878/suppl_file/sc1c00878_si_002.mp4">MP4</a>)This article has not yet been cited by other publications.
chemistry, multidisciplinary,engineering, chemical,green & sustainable science & technology
What problem does this paper attempt to address?