Corrosion Behavior of Pre-oxidized GH4169 Alloy with Solid NaCl Deposited in a Wet Oxygen Flow at 600 °C

Weidong Zhang,Yu Cui,Li Liu,Wenquan Wang,Wenzheng Chen,Rui Li,Fuhui Wang
DOI: https://doi.org/10.1007/s40195-024-01699-9
2024-05-08
Acta Metallurgica Sinica (English Letters)
Abstract:The corrosion behavior of the pre-oxidized GH4169 alloy was studied after 20 h of exposure under a solid NaCl deposit film in a wet O 2 environment at 600 °C by mass-gain measurements, X-ray diffraction, scanning electron microscopy, transmission electron microscopy methods. The results indicate that the pre-oxidized GH4169 alloy undergoes serious corrosion in the corrosive condition. The preformed Cr 2 O 3 layer is gradually destroyed by deposit NaCl, and the inner Nb 2 O 5 layer beneath the complete outer Cr 2 O 3 layer also reacts with NaCl to form NaNbO 3 . The electrochemical test results testified the existence of electrochemical reactions during this corrosion process. The corrosion behavior of pre-oxidized GH4169 under a solid NaCl deposit film in a wet O 2 environment at 600 °C has been discussed in detail.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?