Formation mechanism of interfacial microstructures and mechanical properties of Ti2AlNb/Ni-based superalloy joints brazed with NiCrFeSiB filler metal

Haishui Ren,Xinyu Ren,Weimin Long,Bo Chen,Shujie Pang,Huaping Xiong
DOI: https://doi.org/10.1016/j.pnsc.2020.12.009
2021-04-01
Abstract:Dissimilar joining of Ti<sub>2</sub>AlNb and Ni-based superalloy was successfully conducted using NiCrFeSiB filler metal.The formation of phases Ti<sub>2</sub>Ni (fcc), AlNi<sub>2</sub>Ti (bcc) and TiB<sub>2</sub> (hcp) were confirmed through TEM within the joint.Formation mechanisms of γ solid solution, β<sub>1</sub>-Ni<sub>3</sub>Si, Ni<sub>3</sub>B and CrB phases are discussed.A model of joint microstructural evolution was established.The joint tensile strength at room temperature reached 425 ​MPa and the strength value of 373 ​MPa was maintained at 923 ​K.Dissimilar brazing of Ti<sub>2</sub>AlNb-based alloy and Ni-based wrought superalloy (GH536) was studied using NiCrFeSiB filler metal. The Ti<sub>2</sub>AlNb/GH536 joints were analyzed by scanning electron microscope (SEM) equipped with an electron probe micro-analyzer (EPMA), X-ray diffraction (XRD) and transmission electron microscopy (TEM). The formation mechanism of interfacial microstructure and mechanical properties of Ti<sub>2</sub>AlNb/GH536 joints were studied. The results indicated that Ti<sub>2</sub>Ni(Al,Nb), AlNi<sub>2</sub>Ti and TiB<sub>2</sub> reaction layers were formed in the joint adjacent to Ti<sub>2</sub>AlNb base metal. These layers resulted in high micro-hardness and the weak link of the joint. γ solid solution was formed through isothermal solidification and β<sub>1</sub>-Ni<sub>3</sub>Si phase precipitated in the γ solid solution during cooling process. Ni<sub>3</sub>B, β<sub>1</sub>-Ni<sub>3</sub>Si and CrB phases appeared in the centre of the joint. Blocky and needle-like borides formed within the diffusion affected zone of GH536 base alloy. The maximum tensile strength of Ti<sub>2</sub>AlNb/GH536 joints reached 425 ​MPa ​at room temperature and the strength value of 373 ​MPa was maintained at 923 ​K.<span class="display"><span><ol class="links-for-figure"><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S1002007121000046-fx1_lrg.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download high-res image (451KB)</span></span></a></li><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S1002007121000046-fx1.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download full-size image</span></span></a></li></ol></span></span>
materials science, multidisciplinary
What problem does this paper attempt to address?