Residual Stress Formation and Distortion in Austenitic AISI304 Steel Pipe Weldment with Consideration of Latent Heat using Novel Prescribed Weld Temperature

Pavan Meena,Ramkishor Anant
DOI: https://doi.org/10.1007/s11665-024-09577-2
IF: 2.3
2024-05-26
Journal of Materials Engineering and Performance
Abstract:The utilization of Austenitic AISI304/SUS304/SS304 has become prevalent in the fabrication of superheaters and re-heaters tubes within advanced ultra-supercritical power plants, as well as in pipelines for pressurized heavy water reactor applications, and this choice is primarily attributed to its remarkable corrosion resistance, cost-effectiveness, and superior mechanical properties. The current investigation aims to meticulously examine the applicability of the novel prescribed weld temperature using thermal cycle with moving heat source method for efficiently simulating welding residual stresses formation, distribution, and distortion in 8 mm thick AISI304 steel pipe weldment. Moreover, this study employed latent heat of phase transformation with element birth and death technique in numerical analysis to predict potential issues arising from residual stress in AISI304 pipe weldments. The examination of weldment deformation patterns has revealed that inward bending due to hoop constraint plays a crucial role in preserving dimensional accuracy at the ends of pipes when subjected to axial shrinkage forces. When examining the impact of deformation on the distribution of plastic strain, the calculations reveal that the inner surface of welded pipes experiences significantly higher levels of axial and hoop compressive plastic strain compared to the outer surface. The maximum peaks of von Mises, Tresca, and S33 are observed as 281.8 MPa, 311.9, and 194.6 in the pipe weldment of AISI304 steel.
materials science, multidisciplinary
What problem does this paper attempt to address?