Microstructural analyses of artificial ageing in 5 commercially and non-commercially available Zirconia dental implants

Mona Monzavi,Fei Zhang,Thierry Douillard,Laurent Gremillard,Sammy Noumbissi,Hessam Nowzari,Jerome Chevalier
DOI: https://doi.org/10.1016/j.jeurceramsoc.2020.03.050
IF: 5.7
2020-08-01
Journal of the European Ceramic Society
Abstract:<h3 class="u-h4 u-margin-m-top u-margin-xs-bottom">Objectives</h3><p>The present<em>in vitro</em> study evaluated the effect of LTD (Low Temperature Degradation) on microstructural properties, phase transformation and micro-crack formation of 5 commercially and non-commercially available Zirconia dental implant systems.</p><h3 class="u-h4 u-margin-m-top u-margin-xs-bottom">Methods</h3><p>Accelerated ageing at 134 °C and 2 bar pressure for 30 h was completed. Focused Ion Beam-Scanning Electron Microscopy (FIB/SEM), X-ray diffraction (XRD) and cathodoluminescence quantified phase transformation and micro-crack formation.</p><h3 class="u-h4 u-margin-m-top u-margin-xs-bottom">Results</h3><p>Transformation of the tetragonal grains towards the monoclinic symmetry was observed in all systems. The highest depth was measured in non-commercial TAV dental with the largest grain size (8.7 µm). A micro-cracked layer was associated with the transformation zone. The ageing-related micro-crack formation was parallel to the surface for all groups and was deepest for the non-commercial TAV dental with the largest grain size (7.4 µm).</p><h3 class="u-h4 u-margin-m-top u-margin-xs-bottom">Conclusion</h3><p>LTD following<em>in vitro</em> ageing using an autoclave was minimal for all implant systems investigated.</p>
materials science, ceramics
What problem does this paper attempt to address?