Influences of the pre-oxidation time on the microstructure and flexural strength of monolithic B4C ceramic and TiB2-SiC/B4C composite ceramic

Qi Song,Zhao-Hui Zhang,Zheng-Yang Hu,Shi-Pan Yin,Hao Wang,Xian-Yu Li,Xing-Wang Cheng
DOI: https://doi.org/10.1016/j.jallcom.2020.154852
IF: 6.2
2020-08-01
Journal of Alloys and Compounds
Abstract:B4C is a structural ceramic, which is very sensitive to cracks and flaws. The present study aims to improve its mechanical performance using pre-oxidation process. The monolithic B4C ceramic and TiB2-SiC/B4C (B4C-TSC) composite ceramic were fabricated using spark plasma sintering technique, and they were pre-oxidized at 800 °C in the air. The effect of pre-oxidation time on microstructure and flexural strength was systematically investigated. The results indicated that 30 min was the optimum pre-oxidation time for both B4C ceramic and B4C-TSC ceramic. At this pre-oxidation time, the maximum flexural strength of 601.5 and 785.2 MPa were obtained for B4C ceramic and B4C-TSC ceramic, respectively. The improved flexural strength was primarily ascribed to the formation of glassy oxide layer during the pre-oxidation process and, in turn, the crack healing effect on the surface of the ceramics. Further increasing pre-oxidation time reduced flexural strength due to the pore formation induced by a large amount of CO gas and an intensive evaporation of B2O3 glass phase.
materials science, multidisciplinary,chemistry, physical,metallurgy & metallurgical engineering
What problem does this paper attempt to address?