Enhanced Thermoelectric and Mechanical Performances in Sintered Bi 0.48 Sb 1.52 Te 3 –AgSbSe 2 Composite

Qiang Zhang,Gang Wu,Zhe Guo,Peng Sun,Ruoyu Wang,Lidong Chen,Xuemei Wang,Xiaojian Tan,Haoyang Hu,Bo Yu,Jacques G. Noudem,Guoqiang Liu,Jun Jiang
DOI: https://doi.org/10.1021/acsami.1c05525
2021-05-20
Abstract:Bismuth telluride alloys have dominated the industrial application of thermoelectric cooling, but the relatively poor mechanical performance of commercial zone-melting material seriously limits the device integration and stability. Here, we exhibit synergistically enhanced thermoelectric and mechanical performances of sintered Bi<sub>0.48</sub>Sb<sub>1.52</sub>Te<sub>3</sub>–AgSbSe<sub>2</sub> composites. It is found that the increased hole concentration improves the <i>S</i><sup>2</sup>σ to 40 μW cm<sup>–1</sup> K<sup>–2</sup> at room temperature, and the emerged various defects effectively suppress the <i>κ</i><sub>l</sub> to 0.57 W m<sup>–1</sup> K<sup>–1</sup> at 350 K. All effects harvest a highest <i>ZT</i> = 1.2 at 350 K along with an average <i>ZT</i> = 1.0 between 300–500 K in the <i>x</i> = 0.2 sample. Notably, AgSbSe<sub>2</sub> addition not only optimizes the thermoelectric properties, but also enhances the mechanical performance with a Vickers hardness of 0.75 GPa. Furthermore, the isotropy of thermoelectric properties is also observably promoted by solid-phase reaction combined with high-energy ball milling and hot pressing. Our study reveals a viable strategy to improve the comprehensive performance of sintered bismuth telluride materials.This article has not yet been cited by other publications.
materials science, multidisciplinary,nanoscience & nanotechnology
What problem does this paper attempt to address?