Rapid Fabrication of of Li7La3Zr2O12 Solid Electrolyte with Enhanced Lithium Ionic Conductivity by Microwave Sintering

Yanhua Zhang,Wenjia Luo,Dongwei Hu,Yuxin Deng,Yuan Chen,Jiadong Deng,
DOI: https://doi.org/10.20964/2020.08.67
IF: 1.541
2020-08-01
International Journal of Electrochemical Science
Abstract:Traditional preparation method of solid electrolyte Li7La3Zr2O12 requires a very long sintering holding time (> 36 hours). A efficient and mass production method, microwave sintering, is utilized to prepared LLZO by which the sintering time is reduced to be 2 ~ 4 h. Results show that cubic phase LLZO can be obtained at 1150 oC ~ 1200 oC. With the increase of holding time from 1 h to 4 h, tetragonal LLZO transforms to cubic which suggests extra thermal energy is generated by coupling dielectric loss with microwave. Pellet sintered with 4 h reaches the highest ionic conductivity of 3.1 x 10-4 S cm-1. Long holding time of 6 h will take away a lot of Li from the grain to form excess glass-like phase which is not favorable for conductivity.
electrochemistry
What problem does this paper attempt to address?