Recovery of Phosphate From Industrial Wastewater by Homogeneous Ferrous Phosphate Crystallization and application for synthesis of Lithium Iron Phosphate Battery

Y. Huang,R. Priambodo
2016-07-10
Abstract:This paper studied the recovery phosphate in the form of ferrous phosphate crystal to be re-use as material for synthesis of Lithium iron phosphate (LFP) battery. Phosphorus is a non-renewable resource, it is substantial material in agricultural and industrial applications. Lithium iron phosphate (LFP) is a promising candidate as a cathode material for lithium ion batteries for electric vehicles and stationary electric power storage. In this study, phosphate was crystallized and recovered through homogeneous fluidized bed crystallization (FBC) which was developed from thin film transistor-liquid crystal display (TFT-LCD) Industrial wastewater in Taiwan. TFT-LCD Industrial wastewater containing phosphorus with concentrations 450 ± 10 ppm-P. Ferrous sulfate was used as the precipitant of the phosphorus. Phosphorus removal was initial investigated by using the jar test to know the optimum pH removal, and fluidize bed crystallization (FBC) was used to recover phosphorus wastewater. X-ray diffraction (XRD) analysis suggested that the product recovered was ferrous phosphate crystal. LFP was synthesized from ferrous phosphate combine with Lithium phosphate and ascorbic acid by solid state reaction. Nanopowders and thin films of LiFePO4 have been fabricated and coated on stainless steel substrates with the aim of device development in future. LFP was characterized by (i) TGA/DTG measurement to find optimal calcination temperature, (ii) X-ray diffraction (XRD) for crystal structure, (iii) scanning electron microscope (SEM) for microstructure, (iv) Energy Dispersive X-ray Spectroscopy (EDS) for elemental analysis and (v) FTIR for the internal modes of phosphate ion. Ferrous sulfate was used as precipitant, both of solution introduced at the rate of 30 mL/min and the reflux rate is 150 ml/min. The sample was taken at interval time. Filtered (using 0.45 µm membrane) and unfiltered samples were obtained from the recirculation zone at predetermined time intervals. Both samples were mixed with HNO 3 . The crystals were analyzed by scanning electron microscope (SEM), Energy Dispersive X-ray Spectroscopy (EDS), and X-ray diffraction (XRD). Phosphate and iron concentration was measured by inductively coupled plasma (ICP)
Engineering,Environmental Science,Chemistry,Materials Science
What problem does this paper attempt to address?