A fast and efficient method for selective extraction of lithium from spent lithium iron phosphate battery

Huajian Shentu,Bo Xiang,Ya-Jun Cheng,Tao Dong,Jie Gao,Yonggao Xia
DOI: https://doi.org/10.1016/j.eti.2021.101569
2021-08-01
Abstract:<p>A new recovery method for fast and efficient selective leaching of lithium from lithium iron phosphate cathode powder is proposed. Lithium is expelled out of the Oliver crystal structure of lithium iron phosphate due to oxidation of Fe<span class="math"><math>2+</math></span> into Fe<span class="math"><math>3+</math></span> by ammonium persulfate. 99% of lithium is therefore leached at 40 °C with only 1.1 times the amount of ammonium persulfate without the help of acid treatment. The use of ammonium persulfate also avoids the necessity to remove other metal ions in the later purification process. Various characterization methods including SEM, XPS, XRD are used to explore the experimental leaching mechanism. Theoretical investigations are performed which reveals the E-pH diagram of Fe–P–Li–H<sub>2</sub>O thermodynamic equilibrium. It confirms the possibility and suggests appropriate pH range allowing direct conversion from lithium iron phosphate to iron phosphate with great energy saving and reduced use of acid and base. Based on the experimental and theoretical results, a green and efficient closed-loop recycling route for lithium iron phosphate is proposed.</p>
environmental sciences,engineering, environmental,biotechnology & applied microbiology
What problem does this paper attempt to address?
### What problems does this paper attempt to solve? This paper aims to develop a fast and efficient method for selectively extracting lithium from discarded lithium iron phosphate batteries (LiFePO₄). Specifically, the research addresses the following key issues: 1. **Resource recovery and environmental issues**: - The number of discarded lithium - ion batteries is huge, especially lithium iron phosphate batteries (LFP). Improper disposal of their waste will lead to serious environmental pollution and resource waste. - With the rapid development of electric vehicle technology, a large number of discarded LFP batteries require effective recycling methods to ensure the sustainable use of lithium resources. 2. **Limitations of existing recycling methods**: - **Direct repair method**: Although the waste LFP materials can be restored to new LFP materials by high - temperature sintering, this method is difficult to maintain the consistency of the materials and is prone to introduce impurities, resulting in a decline in electrochemical performance. - **Wet - recycling method**: Traditional wet - recycling usually uses inorganic acids (such as sulfuric acid, phosphoric acid, etc.) to dissolve waste materials. This not only consumes a large amount of acid and alkali but also generates a large amount of wastewater, increasing the treatment cost and environmental burden. 3. **The proposed new method**: - The research proposes a selective leaching method using ammonium persulfate ((NH₄)₂S₂O₈) as an oxidant. By oxidizing Fe²⁺ to Fe³⁺, lithium is released from the olivine structure, thereby achieving efficient selective lithium extraction. - This method avoids the need for acid treatment, reduces the introduction of metal - ion impurities, and is more convenient in the subsequent purification process. 4. **Optimization of reaction conditions**: - By systematically studying various experimental parameters (such as the amount of ammonium persulfate, temperature, reaction time, and solid - to - liquid ratio), the optimal reaction conditions are determined: the temperature is 40 °C, the amount of ammonium persulfate is 1.1 times the theoretical amount, the reaction time is 1 hour, and the solid - to - liquid ratio is 100 g/L. - Under these conditions, the leaching rate of lithium reaches 99%, and the crystal structure and morphology of LFP are not significantly changed. 5. **Closed - loop recycling route**: - Based on the above research results, a green and efficient closed - loop recycling route is proposed. Battery - grade lithium hydroxide is obtained by electrolyzing Li₂SO₄ solution, and ammonium persulfate is regenerated after concentrating the mother liquor, realizing the recycling of reagents. - The finally obtained FePO₄ powder can be used to prepare the original LFP cathode material, thereby realizing the effective recovery of valuable elements in the waste. In conclusion, this research provides an environmentally friendly and economically viable LFP battery recycling method, which helps to promote the sustainable development of the lithium - ion battery industry.