Effects of different elements on the passivation behaviour of Fe-based metallic glasses in the NaCl solution

Haoran Ma,Yanxin Liu,Shuang Zheng,Xiahe Liu,Jiawei Li
DOI: https://doi.org/10.1016/j.apsusc.2023.157805
IF: 6.7
2023-07-01
Applied Surface Science
Abstract:The passivation and microstructure of Fe-based metallic glasses (MGs) with different contents of essential elements in 3.5 wt% NaCl solution were investigated by electrochemical techniques such as potentiodynamic polarization (PDP), potentiostatic polarization (PSP) and Mott-Schottky (MS) as well as surficial stability analysis including X-ray photoelectron spectroscopy (XPS) and ultraviolet photoelectron spectroscopy (UPS). At the low passive potential region, the strongly Cr-enriched passive film on Fe 48 Cr 15 Mo 14 C 15 B 6 Y 2 (Cr 15 Mo 14 ) generates a higher resistance than that of Fe 63 Cr 8 Mo 3.5 C 4 B 4 Ni 5 P 10 Si 2.5 (Cr 8 Mo 3.5 ) with a Fe-rich film. As the potential increases, the enhanced hydration, e.g., Cr 2 O 3 converted to Cr(OH) 3 , causes a film degradation of Cr 15 Mo 14 , while the stable Si-oxide is increasingly enriched and maintains the high film protection of Cr 8 Mo 3.5 . Consequently, the corrosion resistance of Cr 8 Mo 3.5 becomes better than that of Cr 15 Mo 14 at the high passive potential region.
chemistry, physical,physics, applied, condensed matter,materials science, coatings & films
What problem does this paper attempt to address?