In-situ construction of hierarchical cathode electrolyte interphase for high performance LiNi0.8Co0.1Mn0.1O2/Li metal battery

Min Mao,Binhua Huang,Qidong Li,Cuicui Wang,Yan-Bing He,Feiyu Kang
DOI: https://doi.org/10.1016/j.nanoen.2020.105282
IF: 17.6
2020-12-01
Nano Energy
Abstract:High energy density LiNi0.8Co0.1Mn0.1O2 (NCM811)/Li metal batteries exhibit poor cycling due to the inferior structure stability of NCM811. Herein, a hierarchical cathode electrolyte interphase (CEI) with highly dense, resistive and protective properties is in-situ growth on NCM811 by decomposition reaction of lithium difluoro(oxalato)borate (LiDFOB). The hierarchical CEI presents special two-layered structure, where the inner layer is rich in LiF and outer layer mainly contains organic components such as LixBOyFz. The highly resistive inner layer can effectively prevent the NCM811 from further reacting with electrolyte and reduce the accumulation of organic products in outer layer during long cycling. Additionally, the LiDFOB can also induce the uniform deposition of Li ion, increase the Li plating/striping coulombic efficiency and inhibit the growth of Li dendrites. The NCM811/Li battery using LiDFOB presents a greatly improved rate and cycling performance. For instance, the NCM811/Li metal batteries using LiDFOB and LiPF6 based electrolyte delivers a specific capacity of 127.5 and 80.5 mAh g-1 at 10C, respectively and their capacity retentions are 69.8% and 17.1% after 400 cycles. The LiDFOB is a promising lithium salt for advanced high energy density NCM811/Li metal battery.
materials science, multidisciplinary,chemistry, physical,physics, applied,nanoscience & nanotechnology
What problem does this paper attempt to address?
The paper primarily aims to address the issue of poor structural stability in high-energy-density lithium nickel cobalt manganese oxide (LiNi₀.₈Co₀.₁Mn₀.₁O₂, abbreviated as NCM811)/lithium metal batteries during cycling. Specifically: 1. **Poor cycling performance**: The structural instability of NCM811 during long-term cycling leads to poor battery cycling performance. 2. **Electrolyte decomposition**: Highly active Ni⁴⁺ can cause solvent or anion decomposition, thereby affecting battery performance. 3. **Lithium dendrite growth**: The lithium metal anode tends to form lithium dendrites during charge and discharge, which can lead to short circuits or even battery explosions. To address these issues, researchers have proposed an in-situ construction of a hierarchical solid electrolyte interface (CEI) by decomposing lithium difluoro(oxalato)borate (LiDFOB) electrolyte to form a special double-layer CEI structure on the surface of the NCM811 cathode. This CEI features an inner layer rich in LiF and an outer layer rich in organic components, which can effectively protect NCM811 from further reacting with the electrolyte and reduce impedance growth during cycling. Additionally, the LiDFOB electrolyte can induce uniform lithium ion deposition, improve the coulombic efficiency of the lithium metal anode, and suppress lithium dendrite growth. Therefore, this study aims to improve the cycling stability and rate performance of NCM811/lithium metal batteries by enhancing the electrolyte.