Electrochemical and structural characterization of polyacrylonitrile (PAN)–based gel polymer electrolytes blended with tetrabutylammonium iodide for possible application in dye-sensitized solar cells
Faisal I. Chowdhury,Ibrahim Khalil,M. U. Khandaker,M. M. Rabbani,Jamal Uddin,A. K. Arof
DOI: https://doi.org/10.1007/s11581-020-03612-7
IF: 2.961
2020-05-26
Ionics
Abstract:<p class="a-plus-plus">Polyacrylonitrile (PAN)–based gel polymer electrolytes (GPEs) consisting of plasticizers ethylene carbonate (EC) and propylene carbonate (PC) and different compositions of tetrabutylammonium iodide (TBAI) salt have been investigated. The GPEs have been characterized by electrochemical impedance spectroscopy (EIS), linear sweep voltammetry (LSV), and X-ray diffraction (XRD) techniques. EIS study shows that the GPE containing 30 wt% TBAI has the lowest bulk impedance, <em class="a-plus-plus">R</em><sub class="a-plus-plus">b</sub> (23 Ω), and highest room temperature ionic conductivity (3.46 × 10<sup class="a-plus-plus">−3</sup> S cm<sup class="a-plus-plus">−1</sup>). Conductivity-temperature relationship in the temperature range studied obeys Arrhenius rule. The <em class="a-plus-plus">E</em><sub class="a-plus-plus"><em class="a-plus-plus">a</em></sub> value is decreased with TBAI percentage and is the lowest (12.59 kJ/mol) for GPE containing 30 wt% TBAI. From LSV experimental data, the limiting current density (<em class="a-plus-plus">J</em><sub class="a-plus-plus">lim</sub>), apparent diffusion coefficient of triiodide ion (<span class="a-plus-plus inline-equation id-i-eq1"><span class="a-plus-plus equation-source format-t-e-x">\( {D}_{I_3^{-}}^{\ast } \)</span></span>), and exchange current density (<em class="a-plus-plus">J</em><sub class="a-plus-plus">0</sub>) have been calculated. The highest value for each of these parameters is 5.00 mA cm<sup class="a-plus-plus">−2</sup>, 6.59 × 10<sup class="a-plus-plus">−7</sup> cm<sup class="a-plus-plus">2</sup> s<sup class="a-plus-plus">−1</sup>, and 0.63 mA cm<sup class="a-plus-plus">−2</sup>, respectively, for the highest conducting GPE. All samples are amorphous. LSV at stainless steel showed that the electrochemical stability window is 2.2 V. The cyclic voltammetry (CV) was performed from 1 to 1000 cycle which showed good electrochemical stability.</p>
chemistry, physical,physics, condensed matter,electrochemistry