Anisotropic fatigue strength and status of crack initiation of Ti17 disk fabricated by through-transus-processed forging

Wei Chen,Weidong Zeng,Yunteng Xiao,Jianwei Xu
DOI: https://doi.org/10.1016/j.ijfatigue.2023.108117
IF: 5.489
2023-12-24
International Journal of Fatigue
Abstract:The high-cycle fatigue tests were performed along axial direction (AD), radius direction (RD), and inclined direction (ID) of the Ti17 disk fabricated by the through-transus-processed forging. Especially, the elongated β grains exhibits a basket-weave microstructure feature with a wavy grain boundary α. The AD sample presents a minimum fatigue strength. Both the RD sample and ID sample exhibit a maximum and an approximate fatigue strength. The anisotropy of the fatigue strength is determined by the α lath tending to occur basal slip. Meanwhile, the {10 1 ̄ 2} extension twins are observed near the region of the fatigue crack initiation. Besides, the dislocation accumulates at the interface of the α/β phase through the analysis of the Kernal average misorientation and transmission electron microscopy, resulting in that it becomes preferential sites for the fatigue crack nucleation and early propagation.
materials science, multidisciplinary,engineering, mechanical
What problem does this paper attempt to address?