Effect of Milling Time and Reinforcement Volume Fraction on Microstructure and Mechanical Properties of SiCp-Reinforced AA2017 Composite Powder Produced by High-Energy Ball Milling
Shimelis Bihon Gasha,Maik Trautmann,Guntram Wagner
DOI: https://doi.org/10.3390/ma17020435
IF: 3.4
2024-01-17
Materials
Abstract:The influence of milling time and volume fraction of reinforcement on the morphology, microstructure, and mechanical behaviors of SiCp-reinforced AA2017 composite powder produced by high-energy ball milling (HEBM) was investigated. AA2017 + SiCp composite powder with different amounts of SiC particles (5, 10, and 15 vol%) was successfully prepared from gas-atomized AA2017 aluminum alloy powder with a particle size of <100 μm and silicon carbide (SiC) powder particles with an average particle size of 300 nm to 68 nm, 64 nm, and 64 nm after 5 h of milling, corresponding to SiC contents of 5, 10, and 15 vol%, respectively. As a result, the lattice strain increased from 0.15% to 0.5%, which is due to significant plastic deformation during the ball milling process. XRD results showed a rapid decrease in crystallite size during the early milling phase, and the minimum grain size was achieved at a higher volume fraction of SiC particles. Microhardness tests revealed that the milling time has a greater influence on the hardness than the amount of SiC reinforcements. Therefore, the composite powder milled for 5 h showed an average microhardness three times higher than that of other unmilled powder particles.
materials science, multidisciplinary,chemistry, physical,physics, applied, condensed matter,metallurgy & metallurgical engineering