Long‐Term Stability of Ammonia Decomposition over Nickel‐Based Catalysts

Maximilian Purcel,Astrid Sophie Müller,Patrick Diehl,Konstantinos Kappis,Annette Trunschke,Martin Muhler
DOI: https://doi.org/10.1002/ente.202400678
IF: 4.149
2024-04-24
Energy Technology
Abstract:The long‐term stability of a Ni‐based industrial reference catalyst and of a Ni/Al2O3 catalyst prepared by co‐precipitation are investigated in ammonia decomposition at atmospheric pressure. The reference catalyst shows an outstanding stability rendering it suitable for the application in large‐scale plants, whereas the Ni/Al2O3 catalyst suffers from deactivation by sintering. Green hydrogen can be used as the backbone of a novel energy system and as a feedstock for renewable chemistry. H2 storage and transport are challenging, but ammonia as a hydrogen carrier could potentially solve these inefficiencies. Many studies focus on high catalytic activities, but the long‐term stability is often insufficiently investigated. This work reports on the stability of a nickel‐based reference catalyst and a coprecipitated Ni/Al2O3 catalyst over 800 h time on stream (TOS) in 98% NH3 at atmospheric pressure. An automated temperature control is necessary to adjust the temperature of the heat source to compensate for the changing heat demand resulting from catalyst activation or deactivation. Under reaction conditions the reference catalyst first undergo an activation phase before reaching its maximum conversion of 91.9% after 250 h TOS followed by a minor decrease in conversion. In comparison, the Ni/Al2O3 catalyst shows lower activity and undergo a continuous deactivation due to sintering. Overall, the activity loss at 534 °C amounted to only 1.5% for the reference catalyst and to 13.5% for the Ni/Al2O3 catalyst compared with the maximum conversion level. Thus, the Ni‐based reference catalyst proves to be very stable under industrially relevant NH3 decomposition conditions.
energy & fuels
What problem does this paper attempt to address?