Abstract:The MgO–SiO2–H2O binding system was vital for the strength properties of magnesia castables. However, the low yield of magnesium silicate hydrate (M-S-H) during the curing process limited the further improvement in the service performance of magnesia castables. The introduce of synthesized M-S-H into magnesia castables was a potential approach to address the above issue, and it was explored in this work. The effect of dehydration temperature (from 200 to 800 °C) on the rehydration behavior of M-S-H and the strength of magnesia castables was investigated. The results indicated that the magnesia castables with pre-dehydrated M-S-H below 600 °C processed an enhanced binding property. The highest strength occurred in the sample with pre-dehydrated M-S-H at 200 °C, and the strength dramatically decreased in the presence of M-S-H calcinated at 800 °C. According to Molecular Dynamics (MD) simulations, structural distortion was generated from the dehydration process of M-S-H and was worsened by temperature increase. The minimum distortion occurred in the dehydration of M-S-H at 200 °C, which was confirmed as merely 8% physical water removal based on the Density Functional Theory (DFT) calculations. Ultimately, the appropriate structural distortion could increase the hydration reactivity and improve the strength of magnesia castables.
materials science, ceramics
What problem does this paper attempt to address?