Dilatometric study of continuous annealing of a cold‐rolled austenitic stainless steel

Abdelali Hayoune,Halima Maredj,Jamal Fajoui,Pierre-Antoine Dubos
DOI: https://doi.org/10.1002/srin.202300054
IF: 2.1258
2023-06-03
steel research international
Abstract:The sequence of structural changes produced in two deformed microstructures of austenitic stainless steel (ASS) elaborated by a multi‐pass unidirectional cold rolling (CR) and a two‐step one, to a 75 % thickness reduction, was followed by dilatometric experiments. The two materials showed different dilatometric behaviors. XRD and microhardness measurements were performed to underly the observed dilatometric behaviors. The material subjected to multi‐pass unidirectional CR showed an unusual dilatometric behavior. The first heating stage led to the occurrence of the recovery reaction in competition with the ε‐martensite reversion. When the temperature increased between 550 and 780 °C, the reversion of deformation induced α‐martensite took place and led to a complicated dilatometric anomaly. Further increase in temperature led to the occurrence of the recrystallization transformation. However, the material subjected to two‐step CR showed a quite usual dilatometric behavior which was explained by the occurrence of several reactions in the following order: (i) T < 300 °C, the recovery reaction, (ii) 300 < T < 680 °C, the ferro to paramagnetic transformation of α‐martensite, the reversion of ε‐martensite and the athermal reversion of α‐martensite, (iii) 680 < T 760 °C, the recrystallization. This article is protected by copyright. All rights reserved.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?