Effect of zirconium oxide nano-coating on frictional resistance of orthodontic wires

Amin Golshah,Shirin Asadian Feyli,ShirinAsadian Feyli
DOI: https://doi.org/10.4103/jos.jos_154_21
2022-01-01
Journal of Orthodontic Science
Abstract:Objectives: Minimizing the frictional force between orthodontic wire and brackets is imperative to safely obtain a more favorable result by applying lower loads. Several methods have been proposed for this purpose such as changing the wire shape/size, changing the bracket design, and coating wires with different materials. This study aimed to assess the effect of zirconium oxide (ZrO2) nano-coating on frictional resistance of three types of orthodontic wires.Materials and Methods: This in vitro, experimental study evaluated 42 pieces of nickel-titanium (NiTi), stainless steel (SS), and beta-titanium (TMA) orthodontic wires, and 42 maxillary canine brackets. The samples were divided into six groups with and without ZrO2 nano-coating. The nano-coating was applied on the wires using the sol-gel technique. The presence of ZrO2 nano-coating was evaluated by scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDX). The surface roughness of the samples was evaluated using atomic force microscopy (AFM). The brackets and wire had a 5° angle relative to each other. The static and kinetic friction of the samples were evaluated in the presence of artificial saliva and occlusogingival movements in a universal testing machine. Data were analyzed by the Shapiro-Wilk's test, one-way ANOVA, Kruskal-Walli's test, Mann-Whitney U test, independent t-test, and Tukey's test.Results: ZrO2 nano-coating was only observed on TMA wires. The surface roughness of coated NiTi and SS wires had no significant difference from that of non-coated wires (<i>P</i> &gt; 0.05). However, this difference was significant for TMA wires with and without the coating (<i>P</i> &lt; 0.05). The static and kinetic friction were not significantly different between wires with and without coating (<i>P</i> &gt; 0.05).Conclusions: ZrO2 nano-coating could only be applied on TMA wires, and had no significant efficacy for reduction of static or kinetic friction of TMA wires.
What problem does this paper attempt to address?