Effects of particle size distribution and sintering temperature on properties of alumina mold material prepared by stereolithography

Shuang Chen,Chang-Shun Wang,Wen Zheng,Jia-Min Wu,Chun-Ze Yan,Yu-Sheng Shi
DOI: https://doi.org/10.1016/j.ceramint.2021.11.145
IF: 5.532
2022-03-01
Ceramics International
Abstract:Alumina mold materials prepared by stereolithography usually have considerable sintering shrinkage, and their properties related to casting have been rarely studied. In this study, alumina molds materials were prepared by stereolithography, and the effects of particle size distribution and sintering temperature on the properties of the materials were investigated. Results show that the viscosity of the slurries decreases as the fraction of fine powder increases, and the particle size distribution affects the curing behaviors slightly. Sintering shrinkage increases as the fraction of fine powder or the sintering temperature increases. Although lower sintering shrinkage can be achieved by sintering at 1350 °C or 1450 °C, the mold materials sintered at lower temperatures would continue to shrink under the service temperature of 1550 °C, and thus 1550 °C is determined as the optimal sintering temperature. As the fraction of fine powder increases, the creep resistance first increases and then decreases, and specimens prepared with 0.1 fraction of fine powder exhibit the best creep resistance with the droop distance of 4.44 ± 0.45 mm. Specimens prepared with 0.1 fraction of fine powder and sintered at 1550 °C exhibit linear shrinkage of 6.36% along the X/Y direction and 11.39% along the Z direction, and have a flexural strength of 78.15 ± 3.50 MPa and porosity of 30.12 ± 0.08%. The resulting material possesses relatively low sintering shrinkage, proper mechanical strength, porosity and high-temperature properties that meet the requirements for casting purposes.
materials science, ceramics
What problem does this paper attempt to address?