Experimental Study on Surface Microscopic Characteristics of scCO2-MQL Milled γ-TiAl Alloy

Yuansheng Zhai,Jianlun Gao,Yu Wang
DOI: https://doi.org/10.1080/10584587.2024.2322350
2024-10-17
Integrated Ferroelectrics
Abstract:γ-TiAl alloy has high specific strength and excellent low-temperature resistance, but its cutting performance is poor. In this study, the four aspects of residual stress, plastic deformation, surface phase transformation, and work hardening were analyzed via experiments involving supercritical carbon dioxide minimum quantity lubrication (scCO 2 -MQL) and dry milling of γ-TiAl alloy. The results show that the residual stresses generated during the milling process can be significantly improved under the scCO 2 -MQL condition and correspondingly reduced in depth from the surface, while the plastic deformation layer is significantly reduced, and the maximum reduction of β-phase volume fraction is 12.43% under the scCO 2 -MQL condition compared with the dry cutting condition. With increasing cutting speed in the range of 30–90 m/min, the depth of the hardened layer gradually decreased, while increasing the feed rate caused increased microhardness.
engineering, electrical & electronic,physics, condensed matter, applied
What problem does this paper attempt to address?