Study on Preparation of Ceramsite from Shale Slag and Its Application

Changwei Xu,Xinci Deng
DOI: https://doi.org/10.1088/1757-899X/744/1/012026
2020-02-12
IOP Conference Series: Materials Science and Engineering
Abstract:This paper studies the proportion of raw materials and process system for firing shale slag ceramsite. The raw materials and raw material ratio of the shale slag ceramsite were determined by the composition analysis of the shale slag; Through basic experiments, it is concluded that when the proportion of raw materials is shale slag: coal gangue: fly ash: expansion agent = 65 : 16 : 9 : 10. Through optimization analysis, when the tube pressure strength is used as the evaluation index, the optimal plan A2B1C2, the bulk density as the evaluation index, the optimal plan A1B3C2, and the water absorption rate as the evaluation index, the optimal plan A3B1C3. Conclusion: The best sintering system for shale slag granule firing is preheating temperature 50°C. heating time 20min, holding time 15min, heating to 1100°C, heating for 40min, and finally holding for 20min. Through the optimization analysis of the analysis and analysis of variance results, it is known that the firing temperature has the most significant effect on the ceramsite performance.
What problem does this paper attempt to address?