Effect of water-binder ratio on properties of phosphogypsum binder

G Bumanis,J Zorica,D Bajare,A Korjakins
DOI: https://doi.org/10.1088/1757-899X/660/1/012071
2019-12-05
IOP Conference Series: Materials Science and Engineering
Abstract:Technological, physical and mechanical properties of mineral binders are often defined by the amount of water add to the binder known as W/B ratio. The role of water is contributed to the workability of fresh paste, hydration processes, porosity, mechanical performance and durability of the material. Present research summarizes the relationship between gypsum based binder W/B ratio in mixture composition to properties of hardened gypsum binder, giving a marginal borders of properties affected by W/B. The W/B ratios evaluated were from 0.3 to 1.15. Dihydrate phosphogypsum (PG), which is a waste of phosphorus fertilizer industry and commercial gypsum binder were used as a raw material for production of gypsum samples and results compared to commercial gypsum binder. At the beginning PG was dried at 60°C and afterwards homogenized by milling it in ball mill or by collision milling in disintegrator. Samples were made with plasticizers, mineral additives and foam forming additive. In...
English Else
What problem does this paper attempt to address?