Utilization of Silicon from Lemongrass Ash Reinforcement with ADC 12 (Al-Si alloy) Aluminium on Mechanical and Tribological Properties

Palanivendhan Murugadoss,Chandradass Jeyaseelan
DOI: https://doi.org/10.1007/s12633-022-02119-2
IF: 3.4
2022-09-21
Silicon
Abstract:The role of silicon in Al-Si alloy is to enhance its thermodynamic and mechanical properties. Silicon is an eco-friendly source that lowers the melting temperature and enhances the fluidity of alloys. Low-cost synthesis, abundant natural resources, and mass production are other merits of silicon. Silicon possesses excellent properties such as good photoconductivity, ideal thermal expansion, high corrosion resistance, and long-term durability, which improve the system's overall efficiency. In this study, the matrix used in the composite was Al-Si alloy and lemongrass ash (LGA) as the agro-waste reinforcement (2%-10%). The agro-waste composite produced by the stir casting cum squeeze casting method exhibited exceptional physical and tribological characteristics owing to improved bonding between the composite constituents. Thermogravimetric and differential Thermal Analysis (TG–DTA) deduced the maximum weight loss of 81% for the LGA particles. Other tests performed on the composite specimens helped determine the physical, mechanical, tribological, and microstructural properties like density, porosity, hardness, impact, tensile, compressive strength, wear rate, and coefficient of friction. These inferences were compared with ADC12. With the addition of the mass fraction of LGA particles, the density and toughness decreased at the rate of 2.43 g·cm −3 and 11.9 J, respectively. 6% of reinforced LGA particles in the composite have a high hardness of 61.8 HRB and 113 HV, Tensile strength of 192.3 MPa, and Compressive Strength of 535.6 MPa. Further increase in reinforcement reduced the mechanical strength. A linear reciprocating Tribometer (LRT) was used to find the composite's wear rate and friction coefficient. The rate of wear of fabricated composites decreased gradually on adding LGA particles. The composite with 8wt% of LGA reinforcement exhibited a better anti-wear property of 0.0079 mm 3 /m and 0.0084 mm 3 /m on applying a load of 20 N and 40 N. Increasing the reinforcement content reduced the coefficient of friction (CoF) to 0.72 and 0.74 on applying various load. The distribution of reinforcement in the matrix was studied using an Upright Optical microscope (OM) and Scanning Electron Microscope (SEM) with EDAX techniques. Micrographs disclosed the homogeneous distribution and effectively bonded in the composites with a clear interface of LGA reinforcement.
materials science, multidisciplinary,chemistry, physical
What problem does this paper attempt to address?