Biodegradable methylcellulose biopolymer-derived activated porous carbon for dual energy application

Gaurav Nath,Pramod K. Singh,Pawan Singh Dhapola,Tejas Sharma,Girish P. Patil,Chandradip D. Jadhav,Abhimanyu Singh,Subhrajit Konwar,Serguei V. Savilov,Diksha Singh,M. Z. A. Yahya
DOI: https://doi.org/10.1007/s40243-022-00217-0
2022-11-24
Materials for Renewable and Sustainable Energy
Abstract:Activated porous carbon was synthesized from methylcellulose biopolymer through a two-step mechanism involving H 3 PO 4 as an activating agent and then thermally carbonized in a tubular furnace under an inert atmosphere at 850 °C. The product was next rinsed with strong HCl, neutralized with deionized water, and dried in an oven at 80 °C. Then, to fully understand the behavior of the activated porous carbon, it was characterized using techniques such as X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), energy-dispersive X-ray spectroscopy (EDS), RAMAN spectroscopy, Brunauer–Emmett–Teller (BET), and thermal gravimetric analysis (TGA). Additionally, we have created dye-sensitive solar cells and an electric double-layer capacitor (EDLC) using this porous carbon produced from methylcellulose (DSSC). We used the above-mentioned prepared porous carbon for the electrode portion of the Electric Double-Layer Capacitor (EDLC) fabrication, and the maximized polymer electrolyte film made from the methyl cellulose (MC) biopolymer combined with 60 wt.% of 1-ethyl-3-methylimidazolium tricyanomethanide ionic liquid (IL), with a maximum conductivity of 1.93 × 10 −2 S/cm, for the electrolyte. The fabricated EDLC device shows a specific capacitance of 60.8 F/gm at 5 mV/s scan rate which was confirmed by cyclovoltammetry and a low-frequency impedance plot in the CH electrochemical workstation. The DSSC device was fabricated using the same porous carbon as a material for the counter-electrode and the same composition polymer electrolyte that had been used in the EDLC as the electrolyte for the DSSC which yields an efficiency of 0.86%. The fill factor and other parameters were also calculated from the JV characteristics that had been characterized and obtained in the solar simulator.
What problem does this paper attempt to address?