Electrochemical performance and thermal stability of 18650 lithium-ion battery with water mist after high-temperature impact

Jiajia Xu,Lin Zhang,Yujun Liu,Qiangling Duan,Kaiqiang Jin,Qingsong Wang
DOI: https://doi.org/10.1016/j.psep.2022.08.057
IF: 7.8
2022-10-01
Process Safety and Environmental Protection
Abstract:Exposure of LIB to high temperatures may cause certain damage or even fail to work. In this study, the electrochemical performance, the thermal stability and the critical heat of 18650 LIBs with/without water mist after high-temperature impact are experimental investigated. The results demonstrate that water mist raises the critical temperature of battery damage by about 40 °C. With increasing temperature, the electrochemical performance of the battery decreases, primarily caused by loss of lithium-ion. Moreover, water mist also improves the thermal stability of batteries after high-temperature impact, as demonstrated by the higher onset temperature of thermal runaway and activation barriers. Under the use of water mist, the critical heat that the battery performance is not affected and the critical heat for battery damage are obtained based on the increase and distribution of temperature and double integral, which are 2489.46 ± 47.7 J and 4777.63 ± 71.55 J, respectively. This work reveals that water mist could alleviate the damage to the battery caused by high-temperature impact, but when the heat exceeds the critical heat, the damage is irreversible. These findings could provide suggestions for the use of water mist in the thermal safety design of batteries in the future.
engineering, environmental, chemical
What problem does this paper attempt to address?