Thermal Conductivity Switching in Pd-Catalyzed Gd and GdH2 Films Upon Gasochromic Hydrogenation and Dehydrogenation
Riko Hirata,Yuichiro Yamashita,Takashi Yagi,Makoto Kashiwagi,Satoshi Takeya,Yuki Oguchi,Fabio Iesari,Toshihiro Okajima,Naoyuki Taketoshi,Yuzo Shigesato
DOI: https://doi.org/10.1007/s10765-023-03322-y
2024-02-22
International Journal of Thermophysics
Abstract:Thermal conductivity switching in Pd-catalyzed Gd hydride films was investigated using in situ analyses of electrical, optical, structural, and thermophysical properties upon gasochromic hydrogenation/dehydrogenation at room temperature. These reactions allow the films to reversibly switch between the metallic (GdH 2 ) phase in the hydrogenated state and the semiconductor (GdH 3 ) phase in the dehydrogenated state. We fabricated three-layered films comprising Pd (5 nm)/Gd or GdH 2 (300 nm)/Mo (100 nm) using DC magnetron sputtering using Pd, Gd, and Mo targets, respectively, on unheated synthetic quartz substrates. Ar or mixture of Ar + H 2 (H 2 : 5 % to 50 %) gases were used for the deposition of the Gd or GdH 2 films, respectively. The thermal conductivities of the Gd or GdH 2 films were analyzed using in situ rear-heating/rear-detection type time-domain picosecond pulsed light heating thermoreflectance measurements by employing a gas mixture of N 2 /Ar and H 2 (H 2 : 3 %) at 1 atm, which is below the explosive limit for hydrogen. The thermal conductivities of Gd and GdH 2 films were measured for one and two hydro-/dehydrogenation cycles, respectively. The thermal switching ratios of the ON state thermal conductivity to the OFF state thermal conductivity were 6.4 and 2.9–5.4 for the Gd film and the GdH 2 (H 2 : 5 %–50 %) films, respectively. The thermal conductivity of the Gd hydrides films changed along with those estimated from the Wiedemann–Franz Law and electrical conductivities.
thermodynamics,mechanics,chemistry, physical,physics, applied