Laser-Deposited Soft Magnetic Fe–Ni–Mo Alloy: A Processing—Microstructure Study

Samad A. Firdosy,Nicholas E. Ury,Ronald Witt,R. Peter Dillon,Vilupanur A. Ravi
DOI: https://doi.org/10.1007/s13632-022-00819-0
2022-01-28
Metallography, Microstructure, and Analysis
Abstract:High-permeability Ni-15 Fe-5 Mo (wt.%) alloy coupons were produced using a directed energy deposition process with varying laser powers and scan speeds. The microstructure of the as-printed alloy is influenced by the printing parameters, and this influence is perceptible even after heat treatment. Electron backscatter diffraction data showed that the grain sizes in all samples were small near the build plate and increase with distance along the build direction. The average grain size of as-printed coupons decreased with increasing scan speed and lower laser power. Preferred orientation along the <110> family of directions was noted when moderate laser powers and scan speeds were utilized. Annealing resulted in a decrease in average grain size with less texturing and more high-angle grain boundaries.
What problem does this paper attempt to address?