Magnetron Sputtering Silicon Thin Film Electrodes for Lithium-Ion Batteries

E. Evshchik,D. Novikov,A. Levchenko,S. Nefedkin,A.V. Shikhovtseva,O.V. Bushkova,Yu A. Dobrovolsky,E Evshchik,
DOI: https://doi.org/10.20964/2018.03.05
IF: 1.541
2018-03-01
International Journal of Electrochemical Science
Abstract:Thin silicon films were deposited on surface-modified copper foil by magnetron sputtering; Si mass loading varied from 0.013 to 0.400 mg/cm. Scanning electron microscopy (SEM), X-ray photoelectron spectroscopy (XPS), X-ray diffraction (XRD), and transmission electron microscopy (TEM) were used to characterize the structure, morphology, and composition of the Si films as a function of mass loading. It was established that Si films repeated the hill-like morphology of Cu foil surface and consisted of nearly spherical agglomerates of amorphous silicon; the average size and packing of agglomerates varied as the Si mass loading changed. Galvanostatic half-cell electrochemical measurements were carried out within the range of 0.04–2.0 V with a lithium foil as the counter electrode and 1M solution of LiPF6 in 1:1 (v/v) mixture of ethylene carbonate (EC) and diethyl carbonate (DEC) as the electrolyte. According to the results obtained, the highest value of the reversible capacity of about 1200 mAh/g after 50 charge-discharge cycles at 0.1 C was observed in the electrodes with a Si mass loading of 0.293 mg/cm. The non-monotonic dependence of the reversible capacity vs. Si mass loading is likely to be caused by the structural evolution of the amorphous Si thin films.
electrochemistry
What problem does this paper attempt to address?