Porous Ba0.85Ca0.15Zr0.1Ti0.9O3 Ceramics for Pyroelectric Applications

Moolchand Sharma,V. P. Singh,Shatrughan Singh,Puneet Azad,Bouraoui Ilahi,Niyaz Ahamad Madhar
DOI: https://doi.org/10.1007/s11664-018-6375-6
IF: 2.1
2018-05-22
Journal of Electronic Materials
Abstract:Porous Ba0.85Ca0.15Zr0.1Ti0.9O3 (BCZT) ferroelectric ceramics were fabricated using a solid-state reaction consisting of BCZT and poly(methyl methacrylate)(PMMA) (2%, 4%, 8% and 10% by wt.%) as a pore former. By increasing the PMMA content from 0% to 10%, porosity increased from 8% to 29%. It was found that the dielectric constant (εr) decreased and the dielectric loss (tanδ) increased with increasing porosity. At 29% porosity, εr of the BCZT was found to decrease more, from 3481 to 1117 at 5 kHz and at room temperature. The dielectric constant and volume-specific heat capacity decreased with the increase in porosity which ultimately improved the pyroelectric figure-of-merits (FOMs). Further, the pyroelectric FOMs were estimated and found to be improved at optimum porosity.
engineering, electrical & electronic,materials science, multidisciplinary,physics, applied
What problem does this paper attempt to address?