Preparation and application of chelating multi-metal chitosan selenite

X H Zeng,Z Wu,Y C Liu,S M Wen,H M Wang
DOI: https://doi.org/10.1088/1755-1315/185/1/012018
2018-08-30
IOP Conference Series: Earth and Environmental Science
Abstract:[Objective] The aim is to introduce a production processes for the preparation of chelating multi-metal chitosan selenite and its different dosage forms, which is suitable for the fields of food and feed chemistry, fertilizer chemistry or fine chemical technology, and also belongs to the field of biomedical engineering technology. [Method] Disperse chitosan in water, and stir it in water bath at 50-70°C under heating. Add trace elements and rare earth metal salts with matching ratio to make them dissolve, where ratio of chitosan and metal salts is 1:0.1-0.3 (W/W). After 2-5 hours of stirring, chitosan chelated by multi-metal can be obtained. Chelating multi-metal chitosan selenite can be made after adding selenium oxide aqueous solution. [Result] The same molecules of target products produced according to the process contain a variety of metal elements and selenium elements and have biological synergistic effect with its biological solubility and biological activity significantly improved. [Conclusion] Chelating multi-metal chitosan selenite presented in this paper is a kind of trace element and/or rare earth preparation, which is environmentally friendly, easy to absorb and rich in selenium without toxic side effects. Therefore, it could be used as a new preparation to supplement selenium and trace elements in medicine, health care products, cosmetics and agricultural fields.
What problem does this paper attempt to address?