A polymer electrolyte by ozonolysis of poly(3-(trimethoxysilyl) propyl methacrylate) grafted on natural rubber latex in colloid state and its application

Pensiri Silakul,Rathanawan Magaraphan
DOI: https://doi.org/10.1007/s13726-019-00714-6
IF: 2.485
2019-05-13
Iranian Polymer Journal
Abstract:Polar species of natural rubber (NR) core were produced from PMPS-<em>g</em>-NR using ozonolysis. Poly(3-(trimethoxysilyl) propyl methacrylate) (PMPS) coated on NR particles (PMPS-<em>g</em>-NR) was successfully prepared by surface grafting polymerization using a redox couple initiator. PMPS-<em>g</em>-NR was treated by ozone at different feeding rates (50, 75, 100, and 125 mg/h) and treatment times (15, 30, 60, and 120 min) leading to an increase in polar function. Fourier transform infrared spectrometry (FTIR) showed that unsaturated bond (840 cm<sup>−1</sup>) was consumed by ozone resulting in higher intensities of carbonyl and carboxyl groups. The highest percent gel content of ozonized PMPS-<em>g</em>-NR was found at 100 mg/h at each ozone treatment time. After preparation as a polymer electrolyte, the electrical properties were significantly improved. Ozonized PMPS-<em>g</em>-NR showed that the highest ionic conductivity of ozonized PMPS-<em>g</em>-NR was 1.96 mS cm<sup>−1</sup> using an ozone feeding rate of 75 mg/h for 60 min while PMPS-<em>g</em>-NR was 0.41 mS cm<sup>−1</sup>. The solar cell conversion efficiency (<em>ƞ</em>) of ozonized PMPS-<em>g</em>-NR at 75 mg/h for 60 min was 1.51% having a higher value than PMPS-<em>g</em>-NR (0.35%). For thermal stress stability, normalized <em>ƞ</em> value of ozonized PMPS-<em>g</em>-NR remained at 6.25% after 26 days while normalized <em>ƞ</em> of PMPS-<em>g</em>-NR was 27.27% at 22 days and then reduced to an approaching zero value.
polymer science
What problem does this paper attempt to address?