Microstructure, corrosion-resistance, and wear-resistance properties of subsonic flame sprayed amorphous Fe–Mo–Cr–Co coating with extremely high amorphous rate

Chaorun Si,Bingbing Duan,Qi Zhang,Jin Cai,Weichao Wu
DOI: https://doi.org/10.1016/j.jmrt.2020.01.024
IF: 6.267
2020-05-01
Journal of Materials Research and Technology
Abstract:<p>The low-cost Fe-based amorphous coating with the composition of Fe<sub>49.9</sub>Mo<sub>32.9</sub>Cr<sub>9.32</sub>Co<sub>4.55</sub>Si<sub>2.28</sub>Al<sub>1.55</sub> (wt.%) were deposited on 316L stainless steel substrate by subsonic flame spraying under optimum spraying parameters. The microstructure, phase composition, microhardness, corrosion-resistance, and wear-resistance properties of the coatings were systematically investigated. The prepared coating primarily consists of amorphous phase (calculated amorphous phase content was 90.23%), and the hardness of the prepared coating can reach 981.6 HV<sub>0.1</sub>, which is much larger than that of the substrate material 316L stainless steel. The corrosion potential and corrosion current density of the prepared Fe-based amorphous coating in 3.5 wt.% NaCl solution are −438 mV and 6.9 μA/cm<sup>2</sup>, respectively. Compared with 316L stainless steel and some newly published Fe-based amorphous coatings, the prepared coating shows better corrosion resistance properties. The dry sliding wear rate of the coatings with 0.45% C steel balls at 19.6 N is 1.68 × 10<sup>−5</sup> mm<sup>3</sup>/Nm. The friction coefficient of the coating is at an ultra-low level (about 0.26) and can keep relatively steady throughout the sliding test. The study shows that the prepared Fe-based amorphous coating has high amorphous phase content, high hardness, superior corrosion-resistance, and wear-resistance properties.</p>
What problem does this paper attempt to address?