Lightweight AlCuFeMnMgTi High Entropy Alloy with High Strength-to-Density Ratio Processed by Powder Metallurgy

Myoung Jin Chae,Ashutosh Sharma,Min Chul Oh,Byungmin Ahn
DOI: https://doi.org/10.1007/s12540-020-00823-5
IF: 3.451
2020-08-19
Metals and Materials International
Abstract:<span class="a-plus-plus abstract-section id-a-sec1"><p class="a-plus-plus">In this study, we synthesized a new Al<sub class="a-plus-plus">16.6</sub>Cu<sub class="a-plus-plus">16.6</sub>Fe<sub class="a-plus-plus">16.6</sub>Mn<sub class="a-plus-plus">16.6</sub>Mg<sub class="a-plus-plus">16.6</sub>Ti<sub class="a-plus-plus">16.6</sub> lightweight high entropy alloy (LWHEA) by high energy ball milling and spark plasma sintering (SPS). The effect of milling time (15, 30, 45, and 60 h) and SPS conditions (600 and 700 °C) on microstructure, hardness, and density of LWHEAs were studied. The results showed that milled LWHEA is base centered cubic (BCC) structured, consisting of dual BCC1/BCC2 matrix with dispersed minor Cu<sub class="a-plus-plus">2</sub>Mg precipitates and Ti. After SPS of milled samples, the BCC2 phase fraction was increased gradually. The distribution of Ti was uniform up to 45 h milled sample SPSed at 600 °C. However, porosity was built up beyond 45 h milling and higher SPS temperature (700 °C). The presence of finer secondary phases in the HEA matrix contributes to the dispersion hardening. The optimum microhardness and density of LWHEA AlCuFeMnMgTi were around 770 HV and 4.34 g cm<sup class="a-plus-plus">− 3</sup> which is superior to other conventional alloys such as Al or Ti-based alloys.</p></span><span class="a-plus-plus abstract-section id-a-sec2 outputmedium-online"><h3 class="a-plus-plus">Graphic </h3></span>
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?