Preparation of anorthite ceramics using SPS

Štefan Csáki,František Lukáč,Tomáš Húlan,Jakub Veverka,Michal Knapek
DOI: https://doi.org/10.1016/j.jeurceramsoc.2021.03.004
IF: 5.7
2021-07-01
Journal of the European Ceramic Society
Abstract:<p>A mixture of kaolin (92 wt.% of kaolinite) and laboratory-grade CaCO<sub>3</sub> was used for anorthite preparation using the spark plasma sintering (SPS) technique. The powder was heated up to the maximum temperature (850 °C–1100 °C with a step of 50 °C, heating rate 50 °C/min) using the SPS device. The as-prepared samples were compared with a reference sample produced by dry pressing and conventional firing. Rietveld refinement performed on the X-ray diffraction data revealed that before anorthite formation, gehlenite and Ca-feldspar appeared, which gradually transformed into anorthite with increasing temperature. The sample prepared by SPS at 1100 °C contained 90 wt.% of anorthite, while the anorthite content in the reference sample reached only 47 wt.%. The porosity of the samples prepared by SPS reached significantly lower values compared to that of the reference sample. Therefore, SPS can be considered as a promising technique in the preparation of anorthite ceramics at lower temperatures.</p>
materials science, ceramics
What problem does this paper attempt to address?