Fabrication of Nanocrystalline High‐Strength Magnesium−Lithium Alloy by Rotary Swaging

Xin Chen,Chuming Liu,Shunong Jiang,Zhiyong Chen,Yingchun Wan
DOI: https://doi.org/10.1002/adem.202100666
IF: 3.6
2021-08-19
Advanced Engineering Materials
Abstract:A high-strength magnesium-lithium alloy was successfully fabricated via cold rotary swaging in this study. The microstructure evolution in the central and edge regions of the alloy bar during the swaging process was explored using transmission electron microscopy. The results show that nanograins with high-angle grain boundaries can be formed in the central region of the alloy bar after five-pass swaging, resulting in higher microhardness and strength obtained in the central region than in the edge region. The sample in the central region of the five-pass swaged alloy bar exhibited a specific strength of 313 kN m kg-1 and a yield strength of 463 MPa. The nanocrystallization process of initial coarse grains in the central region of the alloy bar contains massive twinning first and subsequent refinement of twin/matrix lamellae through the formation of many dislocation arrays. However, it is not possible to form nanograins in the edge region of the alloy bar after five-pass swaging because of the lower twinning activity and the difficulty of forming dislocation arrays compared with the central region.This article is protected by copyright. All rights reserved.
materials science, multidisciplinary
What problem does this paper attempt to address?