Origin of High Interfacial Resistance in Solid‐State Batteries: LLTO/LCO Half‐Cells**

Pengyu Xu,Wolfgang Rheinheimer,Avanish Mishra,Shoumya Nandy Shuvo,Zhimin Qi,Haiyan Wang,Avinash M. Dongare,Lia A. Stanciu
DOI: https://doi.org/10.1002/celc.202100189
IF: 4
2021-05-11
ChemElectroChem
Abstract:The interface between cathode and electrolyte is a significant source of large interfacial resistance in solid state batteries (SSBs). Spark plasma sintering (SPS) allows densifying electrolyte and electrodes in one step, significantly shorten the manufacturing time, and improve the interfacial contact in SSBs. In this work, we proposed a two‐step joining process to prepare cathode (LiCoO 2 , LCO) / electrolyte (Li 0.33 La 0.57 TiO 3 , LLTO) half cells via SPS. Interdiffusion between Ti 4+/ Co 3+ was observed at the interface by SEM/STEM. Resulting in the formation of Li‐Ti‐La‐Co‐O phase, Li‐Ti‐Co‐O phase in LLTO and Li‐Co‐Ti‐O phase in LCO. Computational modeling has been used to verify that the Li‐Ti‐Co‐O phase has a LiTi 2 O 4 host lattice. In a study of interfacial electrical properties, the resistance of this interdiffusion layer was found to be 10 5 Ω, which is 40 times higher than the resistance of the individual LLTO phase. The formation of an interdiffusion layer is identified as the origin of high interface resistance in LLTO/LCO half‐cell.
electrochemistry
What problem does this paper attempt to address?