Rational Tuning of a Li 4 SiO 4 -Based Hybrid Interface with Unique Stepwise Prelithiation for Dendrite-Proof and High-Rate Lithium Anodes

Yanxia Yuan,Feng Wu,Yiran Liu,Xinran Wang,Ke Zhang,Lumin Zheng,Zhaohua Wang,Ying Bai,Chuan Wu
DOI: https://doi.org/10.1021/acsami.0c12514
2020-08-07
Abstract:Lithium metal batteries (LMBs) are among the most promising candidates for high energy-density batteries. However, dendrite growth constitutes the biggest stumbling block to its development. Herein, Li<sub>4</sub>SiO<sub>4</sub>-dominating organic–inorganic hybrid layers are rationally designed by SiO<sub>2</sub> surface modification and the stepwise prelithiation process. SiO<sub>2</sub> nanoparticles construct a zigzagged porous structure, where a solid electrolyte interface (SEI) has grown and penetrated to form a conformal and compact hybrid surface. Such a first-of-this-kind structure enables enhanced Li dendrite prohibition and surface stability. The interfacial chemistry reveals a two-step prelithiation process that transfers SiO<sub>2</sub> into well-defined Li<sub>4</sub>SiO<sub>4</sub>, the components of which exhibits the lowest diffusion barrier (0.12 eV atom<sup>–1</sup>) among other highlighted SEI species, such as LiF (0.175 eV atom<sup>–1</sup>) for the current artificial layer. Therefore, the decorated Li allows for an improved high-rate full-cell performance (LiFePO<sub>4</sub>/modified Li) with a much higher capacity of 65.7 mAh g<sup>–1</sup> at 5C (1C = 170 mAh g<sup>–1</sup>) than its counterpart with bare Li (∼3 mAh g<sup>–1</sup>). Such a protocol provides insights into the surface architecture and SEI component optimization through prelithiation in the target of stable, dendrite-proof, homogenized Li<sup>+</sup> solid-state migration and high electrochemical performance for LMBs.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acsami.0c12514?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acsami.0c12514</a>.Detailed AFM tests on the Li-SiO<sub>2</sub>-modified Li surface, EIS measurements of symmetric cells with bare Li and Li-SiO<sub>2</sub>-modified Li, SEM images of copper foils after the discharge process, SEM images of the surface morphology and cross-section of the Li-SiO<sub>2</sub>-modified anode and the bare Li anodes (<a class="ext-link" href="/doi/suppl/10.1021/acsami.0c12514/suppl_file/am0c12514_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
materials science, multidisciplinary,nanoscience & nanotechnology
What problem does this paper attempt to address?