Microstructures and Properties of Cu/50 Vol.% MoS2 Composites Prepared with Cu-coated MoS2 Powders and Sintered at Different Temperatures

Ziyan Zhang,Yi Gao,Jinjuan Cheng,Xueping Gan,Chaoqiang Liu,Kechao Zhou
DOI: https://doi.org/10.1016/j.triboint.2024.109967
IF: 5.62
2024-01-01
Tribology International
Abstract:Constitution and distribution of phases and interphase reactions are crucial for properties of composites. So far, the problem of MoS2 agglomeration remains unsolved in Cu/MoS2 composites, and interfacial structures and reaction products between MoS2 and Cu have not been fully considered. Herein, Cu-coated MoS2 powders prepared via electroless plating were sintered at different temperatures into Cu/MoS2 composites. Cu does not react with MoS2 in the composites sintered at 600 degrees C and 650 degrees C, leading to their desirable tribological properties under dry sliding. Reactions between Cu and MoS2 occur in the composites sintered at 700 degrees C and 800 degrees C, and the resultant products include Cu2S, Cu1.8Mo6S8 and Cu1.83Mo3S4 phases, resulting in a better wear resistance under oil lubrication and mechanical properties.
What problem does this paper attempt to address?