Abstract:The Pd/Al2O3-based 2 O 3-based catalysts are highly effective for removing low-concentration methane (CH4), 4 ), a strong greenhouse gas. The sintering of palladium (Pd) particles on the catalysts during long-term utilization causes catalytic deactivation. Magnesium (Mg) promoter would improve the hydrothermal stability of Pd/Al2O3-based 2 O 3-based catalysts by constructing PdO-MgAl2O4 2 O 4 structures on the catalyst surface. In this study, we report an innovative strategy wherein a two-step structure transformation of Mg promoter in a Mg-modified Pd/CeO2-ZrO2-Al2O3 2-ZrO 2-Al 2 O 3 (Pd/CZA) catalyst achieved exceptional hydrothermal stability of the catalyst. The Mg promoter in the form of MgAl2O4 2 O 4 spinel improved PdO reducibility, as indicated by TPR test results, resulting in a 15-17 degrees C decrease in the temperature of 90% CH4 4 conversion (T90) 90 ) over the fresh catalyst. Conversely, the MgO impeded CH4 4 conversion and caused an increased T 90 of 21 degrees C due to forming an electron-rich PdO, as evidenced by XPS and COFTIR test results. Accelerated hydrothermal aging (A) at 800 degrees C for 10 h induced a second structure transformation of MgO to MgAl2O4 2 O 4 in Pd/MgO-CZA catalyst to produce substantial PdO-MgAl2O4 2 O 4 structures, which compensated for the catalytic deactivation caused by the sintering of palladium particles, as demonstrated by XRD, HAADF-STEM, and CH4-TPR 4-TPR test results. As a result, the Pd/MgO-CZA-A exhibited a 13 degrees C decrease in T 90 compared to Pd/MgO-CZA, achieving a T 90 of 425 degrees C with reaction gases containing 10 vol% water vapor. This work provides valuable insights for enhancing the hydrothermal stability of Mg-modified Pd/Al2O3-based 2 O 3-based catalysts.
What problem does this paper attempt to address?