Effects of Two-Step Sub-solution Heat Treatment on Microstructure of New As-Forged Nickel-Based Powder Superalloy Turbine Disc

Liu Zhaofeng,Cheng Junyi,Ma Xiangdong,Xiao Lei,Guo Jianzheng,Feng Ganjiang
DOI: https://doi.org/10.12442/j.issn.1002-185x.20230519
2024-01-01
Rare Metal Materials and Engineering
Abstract:The effect of two-step sub-son heat treatment process on the gamma' phase microstructure of a novel nickel-based powder metallurgy superalloy FGH4113A(WZ-A3) was studied. The results show that the cooling rate of large-size forged turbine dise is lower after forging, and the size distribution of gamma' phases is from about 100 nm to 4500 nm. Small samples were taken from the dise for heat treatment experiments. When the samples are heated to 1000 and 1050 degrees C, the total proportion of gamma' phases decreases, and the evolution mechanism shows signs of Oswald coarsening mechanism and PAM mechanism. When the sample is heated to 1100 degrees C, the intracrystalline gamma' phase is completely dissolved. If two-step sub-solution heat treatment process is used, the sample is first heated to 1120 degrees C for 2 h followed by rapid cooling, and then heated to 1000, 1050 or 1100 degrees C. The total proportion of gamma' phases decreases. The evolution of intracrystalline gamma' phases is dominated by the Oswald coarsening mechanism, and its morphology and size are relatively stable during the beating process. The testing rods were cut from the disc and went through experiments: as-forged state 1000 degrees C (without heat preservation) aging heat treatment and as forged state 1120 degrees C/2 h aging heat treatment. The tensile tests were conducted at 550 degrees C. The yield and tensile strengths of the latter one are significantly higher than those of the first one, and this be treated as a reference for dual-performance heat treatment process design of large-size turbine discs.
What problem does this paper attempt to address?