Study and Analysis on Hot Extrusion Process of High-plastic Magnesium Alloy

Zhang Hu
2014-01-01
Abstract:Hot high-plastic ZK20-0.6Nd magnesium alloys were extruded under different extrusion processes. And the microstructure, DSC(differential scanning calorimetry) curve and tensile properties were tested and analyzed. The results show that as the extrusion speeds increase from 1.5m/min to 6.5m/min, the average grain size of the alloy increases gradually and tensile strength and elongation decrease; as the extrusion ratios increase from 15 to 45, the average grain size decreases and tensile strength and elongation increase. Moreover, the influences of extrusion speed and extrusion ratio on DSC curves of the alloy are unconspicuous and the melting point of the alloy remains at(650±0.5)℃.