Abstract:Through orthogonal tests with three factors,the dielectric properties of CaO-B_2O_3-SiO_2 system glass ceramics are investigated with different conditions of sintering process such as sintering temperature,soaking time,heating speed.The result shows that the optimized condition is 900℃,8℃/min,and 10min.The sample has low dielectric loss and dielectric constant(tgδ=l.81×10~(-4),e=5.6 at 1MHz).XRD,SEM,EDS are used to analyze the crystalline phase and determine the chemical composition.The SEM analysis indicates that the higher sintering temperature increases the crystal size,decreases pores,and reduces dielectric loss.