Pre-Placed Metal Laser-Additive Manufacturing on Grade 5 Titanium Substrate: Layer Formation, Oxidation Resistance, and Wear Resistance

Junyu Lin,Ji Wang,Chang Xu,Benben Li,Bin Chen,Peiquan Xu,Leijun Li
DOI: https://doi.org/10.3390/met13081372
IF: 2.695
2023-01-01
Metals
Abstract:The laser parameters and additive materials were investigated for the laser-additive manufacturing of titanium alloys. A pre-placed metal-strip-based method for 3D printing titanium components was proposed. Before laser processing, the metal strips were fixed to a Grade 5 titanium substrate using resistance spot welding. The effect of the processing conditions (laser power: 1.5-3.0 kW; scanning speed: 3-9 mm center dot s (-1); one or three layers; 1, 6, or 12 passes; Grade 2 and Grade 5 as additives) on the microstructures, oxidation resistance, and wear resistance of the as-printed samples was investigated. The results showed that the microstructure consisted of alpha ' martensite, oxygen-stabilized alpha, transformed beta that contains coarse and fine acicular alpha, titanium oxides, and carbides. Cracks were observed, particularly near the upper surface of the three-layer samples. The cracks were suggested to have formed due to cumulative residual stresses and the formation of oxygen-stabilized alpha and alpha ' martensite that might cause embrittlement. Both oxidation and wear tests were conducted to verify the improved performance. After 55 h of oxidation, the as-printed samples showed mass gains of 0.029-0.035 g center dot cm (-2), which were smaller than those of the substrate (0.039 g center dot cm (-2)).
What problem does this paper attempt to address?