Characterizations on the Microstructures of LiMn{sub 2}o{sub 4} Prepared by a Simple Soft-Chemical Technique

Kwang‐Bum Kim,Gang Chen,Chul W. Park
IF: 4.537
2008-01-01
Materials Characterization
Abstract:LiMn{sub 2}O{sub 4} powders were prepared by a simple soft-chemical technique at different temperatures. X-ray diffraction and thermogravimetric analysis suggested that the material prepared at 800 deg. C was stoichiometric LiMn{sub 2}O{sub 4}, whereas those prepared at 600 and 700 deg. C were Li[Mn{sub 0.77}{sup 3+}Mn{sub 1.23}{sup 4+}]O{sub 4.115} and Li[Mn{sub 0.85}{sup 3+}Mn{sub 1.15}{sup 4+}]O{sub 4.075}. Several typical XRD peaks of the compounds were investigated with an aim to elucidate (i) the Li immigration to the 16d octahedral sites, (ii) the partial tetragonal phase transition of the material and (iii) the mean coherent domain size and microstrain. SEM study showed that the particle size of the materials increased with heating temperature. The activation energy for the material particle growth was determined as 30.4 kJ mol{sup -1}.
What problem does this paper attempt to address?