Enhanced Compatibility, Morphology, and Low-Temperature Toughness of Polyamide 6/poly(dimethylsiloxane)/epoxidized Silicone Rubber Composites

Weizhen Zhang,Zhilong Yang,Yuan Li,Qi Zhang,Shijun Zhang,Liqun Zhang
DOI: https://doi.org/10.1021/acs.iecr.3c00348
2023-01-01
Industrial & Engineering Chemistry Research
Abstract:Epoxidized silicone rubber with an epoxy content of 5%(ESR-5)was introduced to improve the compatibility of the polyamide 6 (PA6)/poly(dimethylsiloxane)(PDMS) composite. The effects of the ESR-5 on the molecular structure,interfacial morphology, and toughness and thermal properties of thePA6/PDMS composite were investigated using nuclear magnetic resonance(NMR) spectroscopy, Fourier transform infrared (FT-IR) spectroscopy,differential scanning calorimetry (DSC), scanning electron microscopy(SEM), atomic force microscopy (AFM), and dynamic thermomechanicalanalysis (DMA). The FT-IR spectra and torque rheological testing confirmedthe reaction between the epoxy group of ESR-5 and the carboxyl groupat the end of PA6. The AFM and SEM images confirmed that the ESR-5altered the interfacial thickness and remarkably decreased the averagesize of the dispersed rubber particles, which enhanced the interfacialcompatibility. At a rubber content of 20% by weight in PA6/PDMS composites,the optimum impact strength at -60 degrees C, which is 469% higherthan pure PA6, was obtained with an ESR-5 content of 50% in rubberphase.
What problem does this paper attempt to address?